ACM, AEM compounding rubber
Product Description
Performance | Brand | |||
AB630 | AB730 | AB830 | ||
Normal performance | Hardness | 60 | 70 | 80 |
Tensile Strength Mpa | 10 | 11 | 10 | |
Elongation at break % | 365 | 270 | 195 | |
Heat aging resistance | Hardness change | +4 | +6 | +5 |
Tensile strength change rate % | 2.0 | 6.8 | 0.7 | |
Rate of change in elongation at break % | -3.6 | -5.4 | -6.3 | |
Resistant to ASTM 1# oil | Hardness change | +0 | +2 | +2 |
Volume change % | -3.3 | -2.1 | -2.7 | |
Resistant to ASTM 3# oil | Hardness change | -10 | -7 | -5 |
Volume change % | +13.6 | +12.2 | +10.8 | |
Compression set % | 26 | 30 | 28 | |
Brittle temperature ℃ | -25 | -25 | -25 | |
Features and uses | Various high temperature resistant oil seals and hoses |