Halogen-free flame-retardant cable jacket compound
TC1202 125℃ Halogen-Free, High-Flame-Retardant Compound
I. Description
This material uses EVM (ethylene-vinyl acetate copolymer) as the base material and is specifically designed for the production of low-smoke, halogen-free, flame-retardant wires and cables. It is widely used in wire and cable companies in European countries such as Germany, the UK, and France, and has the characteristics of being halogen-free, low-smoke, highly flame-retardant, and oil-resistant. Because this material's vulcanization system does not contain free sulfur, it will not react with copper to produce copper sulfide, so the copper wire will not be affected by blackening and its performance will not be affected.
II. Applications
It can be used as insulation for medium and low-voltage wires and cables or as a sheath for other cables. Cables made from this material can be used for a long time at temperatures between -25℃ and 125℃. It is used in the production of motor leads, locomotives, vehicles, subways, oil platforms, ships, nuclear power plant cables, or cables used in similar situations. The material is white, but other colors can be provided according to customer requirements. In addition, this material has high flexibility, which can reduce the bending radius of the cable, making it easier to install and lay.
III. Properties
| Item | Typical Value | Item | Typical Value |
| Original Tensile Strength N/mm2 Elongation at Break % |
11.0 180 |
Oxygen Index % | 45 |
| 158℃ 168h Air Oven Aging Tensile Strength Retention % Elongation at Break Retention % |
110 90 |
PH Value Conductivity μs/mm |
7.2 1 |
| 100℃ 70h Immersion in ASTM #2 Oil Tensile Strength Retention % Elongation at Break Retention % |
70 75 |
Breakdown Voltage KV/mm Volume Resistivity at 20℃ Ω·cm |
22 5×1013 |
| 70℃ 168h Immersion in #0 Diesel Tensile Strength Retention % Elongation at Break Retention % |
60 60 |
Mooney Viscosity 1+4, 100℃ Mooney Scorch ts, 120℃ Vulcanization 180℃ |
55 8.8 15 |
| -25℃ Low Temperature Elongation % | 35 | Specific Gravity g/cm3 Shore Hardness |
1.58 85 |
IV. Processing Technology
It is recommended to use a CV (continuous vulcanization) production line for extrusion production.
Extruder Compression Ratio: 1.1:1~1.5:1 Length-Diameter Ratio: 6:1~16:1
Temperature: 50~70℃
Vulcanization Temperature: The recommended temperature inside the vulcanization pipe should not be lower than 200℃
V. Packaging and Storage
25kg per bag, the material is in the form of a film, and it should be stored in a clean, dry, cool, and ventilated warehouse.
The technical advice provided by our company, whether verbally, in writing, or through testing, is given in good faith, but is not guaranteed. Users are also responsible for testing the products supplied by our factory to verify their suitability for the intended process and application.